Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.02 g/cc | 0.0368 lb/in³ | NCMT Method |
NCMT NanoPAC™ HS404 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Density | 1.02 - 1.43 g/cc | 0.0368 - 0.0517 lb/in³ | Average value: 1.20 g/cc Grade Count:86 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Momentive Performance Materials RTV656 Clear Extreme Low Temperature Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
Multibase Multi-Flamâ„¢ 2602 PP Polypropylene Features:Flame RetardantHalogenatedBlooming, None Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Solvay Chemicals ANTAROX® BL-225 Wetting agent as suspension additivesHS No.: 34021300 /CAS-No.: 68603-25–8 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Solvay ALKAMULS® 696 D Surfactant Description: Ethoxylated castor oil of HLB close to 8, useful as an emulsifier in liquid formulationsIdentification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Available in: Asia Pacific, Eu.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Solvay GEROPON® HW 15 N Surfactant Description: "New ether carboxylate. Based on a fatty alcohol which is commonly available. Emulsifier and lime soap dispersant for metal working fluids."Identification: ALCOHOL ETHO-CARBOXYLATED AC.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | DIN 53479 |
Polyram PlusTek RD104 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Density | 1.02 g/cc @Temperature 260 °C |
0.0368 lb/in³ @Temperature 500 °F |
Melt |
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow.. |
|||
Density | 1.02 g/cc @Temperature 300 °C |
0.0368 lb/in³ @Temperature 572 °F |
Melt |
Covestro Makrolon® 3107 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minGeneral purposeHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpare.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Dow Latex LXC 8437NA Carboxylated Styrene-Butadiene Latex Applications: Latex LXC 8437NA is a versatile residential and commercial carpet latex with a medium hand. Latex LXC 8437NA offers good tuftbind and delamination properties and has exceptional filler.. |
|||
Density | 1.02 g/cc @Temperature 260 °C |
0.0368 lb/in³ @Temperature 500 °F |
Melt |
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content |
|||
Density | 1.02 g/cc @Temperature 280 °C |
0.0368 lb/in³ @Temperature 536 °F |
Melt |
Covestro Makrolon® 2456 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab.. |
|||
Density | 1.02 g/cc @Temperature 280 °C |
0.0368 lb/in³ @Temperature 536 °F |
Melt |
Covestro Makrolon® OD2015 Polycarbonate Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
Diamond Polymers Softflex® 1701-1402 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
Density | 1.02 - 1.06 g/cc | 0.0368 - 0.0383 lb/in³ | Spec; ISO 1183-1 |
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com.. |
|||
Density | 1.02 - 1.06 g/cc | 0.0368 - 0.0383 lb/in³ | Spec; ISO 1183-1 |
Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co.. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | |
BASF Isobutyryl Chloride Formula: C4H7ClOCAS: 79-30-1Description: Isobutyryl chloride is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: Isobutanoyl chloride, Isobutyri.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 415-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foamsApplications: Visible cover pa.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 570 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material .. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D1475 |
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic component.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Peripor® 300 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled Impact modified, injection moldingInformation provided by PolyPlastic Group. |
|||
Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c.. |