Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.980 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
STN EN ISO 1183-1
Plastcom PLASTALEN® PC 69 T 10 003 Polypropylene reinforced with mineral filler
Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o.
Density 0.980 g/cc
0.0354 lb/in³
Premix Thermoplastics PRE-ELEC® PP 1375
PRE-ELEC PP 1375 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE
Information provided by Polykemi AB
Density 0.980 g/cc
0.0354 lb/in³
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183-1
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
Density 0.980 g/cc
0.0354 lb/in³
TPE-0105 (ASTM D792)
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be ..
Density 0.980 g/cc
0.0354 lb/in³
TA4302B
Permabond TA4302 Toughened Acrylic Adhesive
PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Density 0.980 - 1.46 g/cc
0.0354 - 0.0527 lb/in³
Average value: 1.05 g/cc Grade Count:296
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Lucobit Lucolit® 1322 Polyolefin TPO Granules, Red
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of pro..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON MX10301C PP
LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Density 0.980 g/cc
0.0354 lb/in³
Silon Taboradd 23-08350 Processing Aid Masterbatch
Masterbatch with a highly effective processing aid for polyethylene, especially PE-X and PE-HD.Information provided by Silon
Density 0.980 g/cc
0.0354 lb/in³
Solvay ALKAMIDE® AK50BN Surfactant
Chemical Name: TALL OIL DIETHANOLAMIDEINCI NAME: Tallowamide DEACAS: 68155-20-4; 111-42-2; 67-56-1; 61790-12-3Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMID..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Lubrizol Stat-Rite® S-250 Static Control Polypropylene
Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
DuPont Appeel® LSR20D752 Lidding Sealant Resin
Appeel® LSR20D752 is a modified ethylene acrylate copolymer designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Density 0.980 - 1.00 g/cc
0.0354 - 0.0361 lb/in³
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Tipco Tipcolene® FPZ-CL - 10% Talc/Mineral Reinforced Polypropylene Copolymer Compound
10% Mineral Reinforced PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene
Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou..
Density 0.980 g/cc
0.0354 lb/in³
Dow Corning SYL-OFF® PMCPSL 1 Crosslinker
Information provided by Dow Corning
Density 0.980 g/cc
0.0354 lb/in³
Melt
Covestro Desmopan® DP 9650DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedAs of ..
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
ExxonMobil Exxtral™ BMU 130 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe F..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Entec Hypro™ PPC-CC10 Natural Copolymer Polypropylene, 10% Calcium Carbonate Filled
Information provided by Entec
Density 0.980 g/cc
0.0354 lb/in³
ASTM D297
Dow Nordel® NDR 47130.01 EPDM Hydrocarbon Rubber
Description: NDR 47130.01 is a very high molecular weight, semicrystalline EPDM grade with a fast cure rate. It also offers an excellent combination of:very fast mixing with good dispersion levelexc..
Density 0.980 g/cc
0.0354 lb/in³
BASF Benzylamine
Formula: C7H9NCAS: 100-46-9Description: Benzylamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: (Aminomethyl)benzene, BenzenemethanaminApplications: I..
Density 0.980 g/cc
0.0354 lb/in³
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Density 0.980 g/cc
0.0354 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..