Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
SABIC B4660/B4660AB High Density Polyethylene for Blow Molding Product Description: B4660 series grades are medium molecular weight High Density Polyethylene homopolymer for blow molding applications. They are primarily designed for imparting high rigidity, t.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
SABIC F04660 High Density Polyethylene for Blown Film Applications Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness.Applications: Tote boxes, beverage crates.Data provided by the manufacturer. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2908C HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughnessApplications: Tote boxes, Beverage cratesAdditives: AntioxidantInformation provided by NOVA Chemicals. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
Petromont 1100 High Density Polyethylene Resin Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous b.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
Petromont 2200 High Density Polyethylene Resin Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring impr.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
Petromont 8001 High Density Polyethylene Resin Pétromont HDPE 8001 is a high density, homopolymer polyethylene resin produced using the UNIPOL® Process. This high strength resin is intended for extrusion on cast line, where excellent processab.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
SABIC BM6246LS High Density Polyethylene for Blow Molding Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ISO 1183 |
Total Lacqtene® 2007 TN 61 HDPE pipe
(discontinued **) LACQTENE® 2007 TN 61 is a high density homopolymer polyethylene produced by the gas phase polymerization process.LACQTENE® 2007 TN 61 is best processed between 190 and 230°C.Information provided .. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M6138 High Density Polyethylene ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness... |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
Global MB-6366 High Density Polyethylene Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D4883 |
Ineos J60-800-178 HDPE A high density polyethylene homopolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still and sparkling water.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D4883 |
Ineos T60-500 HDPE T60-500 is a high density polyethylene homopolymer designed specifically for injection molding. This narrow molecular weight distribution resin is a product of Ineos USA, LLC's innovative technolog.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D4883 |
Ineos T60-800 HDPE Ineos T60-800 is a high density polyethylene homopolymer. This narrow molecular weight distribution resin is a product of Ineos' innovative technology. Parts fabricated from this material exhibit .. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | Calculated from weight of 90 oz/sy |
Mid-Mountain Materials ARMATEX® SF90 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | Calculated from weight of 36 oz/sy |
Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | |
Saint-Gobain Chemfab® 3 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MB/ML 61 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D 792 |
Total 6410 HDPE Film Resin Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HTA 108 High Density Polyethylene Resin Product Description: HTA 108 is a homopolymer HDPE film grade designed to improve stiffness and barrier in coextrusion or in PE blends. When blended with LLDPE, HTA 108 improves their processability.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HYA 800 High Density Polyethylene Resin Product Description: HYA 800 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal .. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D792 |
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE) Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D792 |
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDH-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In a.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | |
BNZ Materials Marinite® P High Temperature Structural Insulation Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM-D792 |
Braskem GD5160 HDPE Blow Molding Polyethylene Homopolymer GD5160 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance and productivity. It was developed for the blow-molding segment. It is used in .. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM-D792 |
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0339C10L Calcium Reinforced |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® D916-39 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, high stiffness, superior strength, gel free, excellent UV resistance.Applications: Industrial woven bags, tarpaulins.Data provided by th.. |