Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Polymer Industries Densetec HDPE Playground Board The versatile properties of Densetec Playground Board make it virtually vandal resistant. The UV stabilizers added to the material make the colors fade-resistant and the standard properties of the H.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D 792 |
NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin HB-W555-EC complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolo.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Petromont 5000 High Density Polyethylene Resin Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
Polikim ULPOLEN® 1000 UHMWPE, Oil The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corner.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Polymer Industries Densetec HDPE Arena Board Densetec Arena Board is ideal for hockey rink applications including dasher boards, kick plates and official lines. Densetec Arena Board exhibits the properties of high impact strength, abrasion-res.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL5505 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight CopolymerApplications: 55 gallon drums (even those with demanding built-in handling rings), industrial tanksFormolene HL5505 is intended for large part blow molding appli.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
Global G-2855 High Density Polyethylene, Blow Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Braskem BT 100K HDPE Blow Molding Polyethylene
(discontinued **) Applications: Large containers from 60 to 200 litersInformation provided by Braskem |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D4883 |
Ineos B53-35H-011 HDPE Ineos B53-35H-011 is a high density polyethylene copolymer developed for blow molding applications. This product is recommended for use in applications which require a combination of high top load .. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D4883 |
Ineos HP55-25-155 HDPE A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require ex.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) HB5510 High Density Polyethylene HB-5510 is a high molecular weight high density polyethylene.Applications: extrusion large blow moldings, jerry cans, film and blown bags.Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
Techmer ES HiFill® HDPE UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5403 EA HDPE Blow Molding Applications:Blow molded containers up to 30 liters for packagingChemicalsHousehold productsOils and foodstuffsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemi.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
Techmer ES HiFill® HDPE Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding Applications:Blow molded containers up to 30 liters for packagingChemicalsHousehold productsOils and foodstuffsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemi.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D 792 |
Total 5502 BZ HDPE injection blow molding Applications: Cosmetics and toiletries, pharmaceuticals, specialty containers, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atof.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HB5502A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5502A is designed for applications requiring excellent stiffness and stress crack resistance properties. It.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
Entec Hypel® PEHD.3/.955 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Diamond Polymers NPP50-0355 High Density Polyethylene Blow Molding/Extrusion Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM-D792 |
Braskem GM5010T2 HDPE High Density Extrusion Polyethylene GM5010T2 is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes. It is produced with bimodal technology and has high molar mass. It shows high mechanical.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM-D792 |
Braskem GM8250T HDPE High Density Extrusion Polyethylene GM8250T is a high-density polyethylene specially developed for the manufacturing of corrugated pipes. It has high molar mass and shows excellent tenacity, high stiffness, good impact resistance, and.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D-1505 |
Bapolene® 2040 Polyethylene, Blow Molding Bapolene 2040 is a copolymer high density polyethylene resin that offers superior modulus, topload resistance and ESCR. It complies with US FDA 21CFR177.1520.Applications: Hot-fill articles, contai.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D 792 |
Total Finathene® RS 528 HDPE blow molding
(discontinued **) Applications: Bleach and detergents, industrial chemicals, industrial parts, cosmetic bottles, food packaging.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
Total Lacqtene® 2001 TBK 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and .. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | Black; ASTM D1505 |
Formosa Plastics Formolene® HP4306 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for l.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 002955 Phillips Process Hexene Copolymer PRIMATOP HDPE 002955 has a high melt strength, excellent stiffness, and excellent stress crack resistance. Applications include large part blow molding resin and sheet extrusion thermoforming.Former.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 003955BAS Hexene Copolymer HDPE 003955BAS features excellent stiffness, stress crack resistance properties, and antistat. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part.. |
|||
Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HB5502B2 Blow Molding HDPE Hexene CopolymerApplications: Pharmaceutical Packaging; Personal Care Products;
Bleach and Detergents Industrial; and Chemicals & PartsFormolene® HB5502B2 is designed for applications requiring ex.. |