Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-4052 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9035 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM 5202 Polyethylene, Sheet/Thermoforming Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D 792 |
Total Finathene® CD 522 HDPE corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® LH5240 Injection Molding HDPE
(discontinued **) CopolymerApplications: Thin wall containersInformation provided by Formosa Plastics Corporation, USA. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
LyondellBasell Lupolen® 4152 D SW 00413 HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.Data was collected by ISO methods and o.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Density | 0.952 - 0.956 g/cc | 0.0344 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HD 7255 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
JPJ Technologies 6100M HDPE Extrusion Information provided by JPJ Technologies |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® BB 85 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® TB 38 HDPE Made for tape applications.Information provided by Unipetrol RPA |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D 792 |
Total 5202LD HDPE, blow molding Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 53600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Housewares.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 755.CM Molding, extrusion and compounding resin Escorene Ultra LD 755.CM is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & M.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HD 6719.17 Injection Molding Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HD 6719.62 Injection Molding Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HTA 002 High Density Polyethylene Resin Product Description: HTA 002 is a general purpose medium molecular weight HDPE grade, characterized by easy processability, especially in coextrusion and blending with other polyolefins. HTA 002 can.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
Dow DMDA-8980 NT 7 High Density Polyethylene Resin DOW DMDA-8980 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
Dow DOWLEX™ IP-60 High Density Polyethylene DOWLEX® IP-60 resin is an improved processing high density polyethylene resin designed to offer excellent processability, good impact and top load strength required in thin wall injection molding. .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0437C10L1 Calcium Reinforced |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® LH5212 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, buckets, housewares, cartridges, closures, toysFormolene LH5212 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Foo.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 055952 Injection Molding Polyethylene HDPE 055952 features maximum toughness, good top loading capability, and high surface gloss. Applications include pails and beverage crates.Former A-Top Polymers product; part of Amco product line s.. |