Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 56B4 HDPE Blow Molding Resin Extra-high stress crack resistance, Good processabilityApplications: Very high ESCR, Ideally suited for use in most food, pharmaceutical, households and industrial chemical applications, Little/no s.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D4883 |
Eastman M30033-P Voridian Polyethylene
(discontinued **) VORIDIAN M30033-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M30033-P has been found to exhibit good barrier properties, tempe.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.2% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7720 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® MV-02520 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An experimental, very high flow, 20% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 8504 BK, 8504 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1475 |
Humiseal 1C51 Silicone Conformal Coating Humiseal 1C51 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1475 |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D4883 |
Ineos A4040 HDPE Ineos HDPE A4040 is a high density polyethylene copolymer produced using a supported catalyst process. It is a copolymer resin used mainly for the extrusion of crosslinked pipes according to the sil.. |
|||
Density | 0.947 - 0.953 g/cc | 0.0342 - 0.0344 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HE 7250 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
Micropol Isoplas P471 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Density | 0.947 g/cc @Temperature 20.0 °C |
0.0342 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell DPM Dipropylene glycol methyl ether Information provided by Lyondell. |
|||
Density | 0.947 - 0.953 g/cc | 0.0342 - 0.0344 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE) DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM-D792 |
Braskem GM5010T2B HDPE High Density Extrusion Polyethylene GM5010T2B is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
Axion Polymers Axpoly® HDPE21 1000 High Purity Molding Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin re.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
BASF Cyclopentanone Formula: C5H8OCAS: 120-92-3Description: Cyclopentanone is a water-white liquid, soluble in water, alcohol and ether.Applications: Intermediate used in the production of pharmaceuticals, biologicals,.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
3M Hi-Strength 94 ET Adhesive A high performance, industrial grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of substrates including decorative laminate, headliners, and soft .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Part B |
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2607-UV9 HDPE Injection Molding Resin
(discontinued **) Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | AboCure 7606-1 |
Abatron AboCast/AboCure 7606-1 Epoxy AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight o.. |