Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.929 - 0.933 g/cc | 0.0336 - 0.0337 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4131L (314F4) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.929 - 0.933 g/cc | 0.0336 - 0.0337 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D792 |
M. Holland Company LL800 LLDPE
(discontinued **) Features: Fast Production Cycle, High Gloss, Low Temp. Impact Resistance, Low to No Odor, Low WarpageUses: Containers, Household Goods, Lids, Thin-walled PartsApprovals: FDA 21 CFR 177.1520(c) 3.2a .. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ExxonMobil Method |
ExxonMobil LD 117.03 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ExxonMobil Method |
ExxonMobil LD 117.08 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ISO 1183 |
Yparex 8125 Polyolefin Adhesive Resin The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Eastman 5251 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent adhesion, Excellent processability and bubble stability, High slip and antiblock, Good impact strengthApplications:Laminations, Heavy produce and s.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | |
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | |
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | |
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Density | 0.929 - 0.933 g/cc | 0.0336 - 0.0337 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | |
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | Fired Density at 2300°F |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M77 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation. Availability: Africa & M.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ExxonMobil Method |
ExxonMobil LD 117.85 Blown Overwrap Film Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade) Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D792 |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
Density | 0.929 g/cc | 0.0335 lb/in³ | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 1000, AGMA Number 8A EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D792 |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM-D792 |
Braskem TX9003 LDPE Blown Film Extrusion Polyethylene TX9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance, good optical properties, and high stiffness. These characteristics provide, in some applications, down gaug.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | |
Arkema Group Evatane® 1010 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, transparent films with high mechanical properties. Examples: stretch film, food packaging.ISO data provided by t.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | |
Arkema Group Evatane® 1090 VN 3 Ethylene Vinyl Acetate Description: EVA copolymer made by high pressure tubular process.Applications:Grade for molding flexible articles.Examples: Closures, plugs, swimming flippers, toys.ISO data provided by the manufact.. |
|||
Density | 0.929 - 0.938 g/cc | 0.0336 - 0.0339 lb/in³ | Average value: 0.934 g/cc Grade Count:21 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE
(discontinued **) Puncture value is 50 J/mm. Hexene LLDPE. Excellent puncture resistance, good stiffness and machinability, and good tensile properties. Additive Package: High slip and antiblock, process aid.Applic.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | |
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Density | 0.929 g/cc | 0.0336 lb/in³ | ASTM-D792 |
Braskem TS9003 LDPE Blown Film Extrusion Polyethylene TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packag.. |