Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.928 g/cc | 0.0335 lb/in³ | Exxon Method |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Injection Molding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be injection molded to produce pliable parts. It can also be used for making.. |
|||
Density | 0.928 - 0.932 g/cc | 0.0335 - 0.0337 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4431S (30405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Eastman 5272 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, Medium antiblock, Medium slip, Good low temperature properties, Good heat seal char.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Eastman 5274 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, High antiblock, Medium slip, Good low temperature properties, Good heat seal charac.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D792 |
DuPont Appeel® LSR11N704 Lidding Sealant Resin
(discontinued **) Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D792 |
DuPont Appeel® LSR11D704 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D2839/D1505 |
ExxonMobil Escorene® FL 00111 Film Resin
(discontinued **) FL 00111 is a copolymer of ethylene and vinyl acetate.Information provided by ExxonMobil Chemical |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |
|||
Density | 0.928 - 0.950 g/cc | 0.0335 - 0.0343 lb/in³ | Average value: 0.938 g/cc Grade Count:30 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
LyondellBasell Lupolen® 3020 D LDPE Blow molding, injection molding.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
LyondellBasell Lupolen® 3020 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
LyondellBasell Lupolen® 3024 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
LyondellBasell Lupolen® 3026 F LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
LyondellBasell Lupolen® 3032 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ISO 1183 |
Borealis Himod™ FT3280 LDPE for Film Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D792 |
DuPont Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00909 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00909 is used in extrusion coating, cast film and co-extrusion. FL 00909 is good sealing material with good optical properties.Processing Conditions: Excellent results are ob.. |
|||
Density | 0.928 g/cc @Temperature 15.6 °C |
0.0335 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Exterex™ A32 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | ASTM D792 |
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA) AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional .. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
BASF Dipropylene Triamine Formula: C6H17N3CAS: 56-18-8Description: Dipropylene triamine is a colorless to yellow liquid with an amine-like odor. Synonyms: Dipropylenetriamine, N-(3-Aminopropyl)-1,3-propanediamine, 1,5,9-Tria.. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
BASF Lucalen® A 3110 M Q 244 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.928 g/cc | 0.0335 lb/in³ | |
Arkema Group Evatane® 1005 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent film with high strength, shrinking at low temperature. Examples: curtain stretch, coextrusion, .. |
|||
Density | 0.928 - 0.932 g/cc | 0.0335 - 0.0337 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) Arak 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.928 - 0.932 g/cc | 0.0335 - 0.0337 lb/in³ | ASTM D792 |
Iran Petrochemical (PCC) Tabriz 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |