Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM112-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil Method |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | Yield Density |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5020 400 Micron LDPE Powder Description: ICOFLO 510-5020 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5023 400 Micron LDPE Powder Description: ICOFLO 510-5023 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5057 80 Micron LDPE Powder Description: ICOFLO 510-5057 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5063 800 Micron LDPE Powder Description: ICOFLO 510-5063 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5019 300 Micron LDPE Powder Description: ICOTEX 520-5019 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5062 500 Micron LDPE Powder Description: ICOTEX 520-5062 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5064 1200 Micron LDPE Powder Description: ICOFLO 510-5064 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc @Temperature 121 °C |
0.0330 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 0.913 - 0.919 g/cc | 0.0330 - 0.0332 lb/in³ | ASTM D4883 |
Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 1520F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 613A Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D792 |
Ensinger TECAFINE™ PP Polypropylene (PP) TECAFINE™ PP is an anti-stated, polypropylene, random copolymer polyolefin engineering plastic providing excellent chemical resistance and high purity. FDA compliant with better mechanical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow AFFINITY™ SM 1350 Polyolefin Plastomer AFFINITY® SM 1350 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in durable injection molded housewares and compression molded closure liners or gaskets. It exhibit.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4701 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4701 copolymer is an ultra low density polyethylene having high pinhole and puncture resistance, tear strength and high impact resistance combined with improved softness. It has low levels .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM C134 |
BNZ Materials BNZ-26 HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.913 - 1.19 g/cc | 0.0330 - 0.0430 lb/in³ | Average value: 0.940 g/cc Grade Count:29 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |
|||
Density | 0.913 - 0.945 g/cc | 0.0330 - 0.0341 lb/in³ | Average value: 0.935 g/cc Grade Count:49 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |