Zeon Chemicals Sivic® Z711 Polyblend Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Sivic®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Sivic® Z711 Polyblend Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sivic Z711 is a fully fluxed polyblend of 28% ACB NBR/PVC (70/30). It is produced via a mechanical technology, which provides a lump-free homogenous polymer.Low ACN base polymer, good extrudability and cold flex properties. Used for industrial and automotive cable and hose applications.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Mooney Viscosity 62 - 74

@Temperature 100 °C
62 - 74

@Temperature 212 °F
(1+4)
Descriptive Properties Value Comments
Bound ACN (%, acrylonitrile) 28
NBR/PVC Ratio 70/30
Type PB