Zeon Chemicals Nipol® 9040 Polyblack Masterbatch

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 9040 Polyblack Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended for use in mechanical goods requiring medium-high solvent and oil resistance. Based on Nipol 35-8 with 50 phr of N550 black.Recommended for use in molded goods requiring high tensile, solvent and oil resistance.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 40
Hot/Cold C
Nipol Base Polymer 40-5