Zeon Chemicals HyTemp® AR12 AR Super ACM Polyacrylate Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® AR12 AR Super ACM Polyacrylate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Curesite is optimized for improved long-term heat and compression set resistance over traditional acrylates with good low-temperature properties.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mooney Viscosity 30 - 36

@Temperature 100 °C
30 - 36

@Temperature 212 °F
(1+4)
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Gehman T100
Descriptive Properties Value Comments
% Volume Swell 30
Curesite Proprietary