Wellman PermaClear™ HP806 (0.84 IV) PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Wellman
Trade Name PermaClear™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman PermaClear™ HP806 (0.84 IV) PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PermaClear® HP806 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.84 IV. PermaClear® HP806 may be used in contact with food in full compliance with the Federal Food, Drug, and Cosmetic Act and applicable food additive regulations including 21 CFR Section 177.1630.Information provided by DAK Americas. Wellman is a subsidiary of DAK Americas.
Physical Properties Metric English Comments
Bulk Density 0.897 g/cc
0.0324 lb/in³
Nominal
Viscosity Measurement 0.82 - 0.86
0.82 - 0.86
[dL/g], Intrinsic; BD-61201-1
Thermal Properties Metric English Comments
Melting Point >= 240 °C
>= 464 °F
BD-61305
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Chip Size 0.24-0.44 gm/20 chips
BD-61223
Color -4.5-0
b*, BD-6600
77-81
L*, BD-6600
Compounds <2 ppm
Acetaldehyde, Measured on chip, BD-61301