Weartech International WT-6H Cobalt Hardfacing & Wear Resistant Alloy

Category Metal , Nonferrous Metal , Cobalt Alloy
Manufacturer Weartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Weartech International WT-6H Cobalt Hardfacing & Wear Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: engine valves, pump shafts & sleeves, hot cutting & rotary knives, high pressure high temperature valves, extrusion screwsInformation provided by Weartech International
Mechanical Properties Metric English Comments
Hardness, Rockwell C 42 - 48
42 - 48
Component Elements Properties Metric English Comments
Carbon, C 1.3 %
1.3 %
Chromium, Cr 30 %
30 %
Cobalt, Co 59.9 %
59.9 %
Iron, Fe 1.0 %
1.0 %
Nickel, Ni 1.0 %
1.0 %
Silicon, Si 1.3 %
1.3 %
Tungsten, W 5.5 %
5.5 %