Weartech International NOREM 04B Iron Hardfacing & Wear Resistant Alloy

Category Metal , Ferrous Metal
Manufacturer Weartech
Trade Name NOREM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Weartech International NOREM 04B Iron Hardfacing & Wear Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: for cobalt-free components in nuclear applications, valvesInformation provided by Weartech International, Norem is a registered trademark of Electric Power Research Institute
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32 - 36
32 - 36
Component Elements Properties Metric English Comments
Carbon, C 1.1 %
1.1 %
Chromium, Cr 22.5 %
22.5 %
Iron, Fe 62.6 %
62.6 %
Manganese, Mn 4.5 %
4.5 %
Molybdenum, Mo 1.9 %
1.9 %
Nickel, Ni 4.5 %
4.5 %
Nitrogen, N <= 0.10 %
<= 0.10 %
Silicon, Si 2.8 %
2.8 %