Wall Colmonoy COLMONOY® 83 PTA - Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide

Category Metal , Metal Matrix Composite , Nonferrous Metal , Nickel Alloy , Tungsten Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name COLMONOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy COLMONOY® 83 PTA - Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description and Application: A tough nickel-chromium-tungsten-boron matrix alloy containing chromium carbides with the addition of extremely hard tungsten-carbide particles for excellent abrasive wear protection. Excellent edge retention. Specifically for plasma transferred arc (PTA) application. Information provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 11.78 g/cc
0.4256 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 43 - 48
43 - 48
single pass
50 - 55
50 - 55
double pass
Component Elements Properties Metric English Comments
Boron, B 0.90 %
0.90 %
Carbon, C 2.0 %
2.0 %
Chromium, Cr 20.3 %
20.3 %
Iron, Fe 1.4 %
1.4 %
Nickel, Ni 40 %
40 %
As Balance
Silicon, Si 1.4 %
1.4 %
Tungsten, W 34 %
34 %
Processing Properties Metric English Comments
Processing Temperature 1120 °C
2040 °F
fusing temperature