Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® F807 Grey Polyetheretherketone (PEEK) Liquid Dispersion

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® F807 Grey Polyetheretherketone (PEEK) Liquid Dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VICOTE® is the brand name for the Victrex range of coatings. VICOTE Coatings are available through Victrex plc or its preferred coater network. The VICOTE F807 Grey grade has been specifically formulated to provide a resilient coating with high wear and abrasion resistance combined with excellent release properties on ferrous substrates such as carbon and cast steels. These properties are retained at high temperatures where other release coatings would potentially fail. VICOTE dispersions have a low level of extractables.VICOTE Coatings have excellent chemical resistance.Information Provided by VICTREX®
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc

@Temperature 25.0 °C
1.10 g/cc

@Temperature 77.0 °F
ISO 2811
Solids Content 25.6 %
25.6 %
theory volume
39 %
39 %
weight; Victrex Internal Test Method
pH 10
10
Victrex Internal Test Method
Viscosity Measurement 17
17
[seconds]; Test Method: BS EN ISO 2431 Din 6 Cup; @ 25°C
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 2kg, Indent 5mm; ISO 6272
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC