Unitika elitel UE3400 Polyester, Flake

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Unitika
Trade Name elitel
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika elitel UE3400 Polyester, Flake.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastomer, Rubber elasticity, Wide compatibility, Low temperature flexibilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders, and modifying agents to the products in new-generation high-tech fields.Characteristics:l products have superior adhesiveness and coatability. They exhibit excellent adhesiveness and coatability to films and molded products of plastic materials such as polyester, polyvinylchloride, polycarbonate, and cellulose acetate; steel materials such as steel plates; metal materials such as copper, and aluminum; woven or nonwoven fabrics from polyester and other fibers; papers, woods, and others.l products may be hardened by combined use of a hardening agent.Blending of an l resin with another l resin or a different resin provides alloys with more diversified resin properties. Additionally, l products are effective as a modifying resin for providing other resins with flexibility, coatability, toughness, and others. l resins form films excellent in flexibility, electrical properties, weather resistance, as well in appearance and transparency: l resins retain consistent quality with smaller change in quality over time They are also excellent hygienically.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
JIS K-6911
Moisture Absorption at Equilibrium 0.50 %
0.50 %
60%RH
Viscosity 50 cP

@Temperature 200 °C
50 cP

@Temperature 392 °F
Melt
Viscosity Measurement 0.92
0.92
Limiting Viscosity
Molecular Weight 25000 g/mol
25000 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 28
28
Tensile Strength at Break 2.00 MPa
290 psi
ASTM D638
Elongation at Break 1400 %
1400 %
ASTM D638
Thermal Properties Metric English Comments
Softening Point 105 °C
221 °F
JIS K-2531
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
Electrical Properties Metric English Comments
Dielectric Constant 5.3
5.3
ASTM D150
Dissipation Factor 0.030
0.030
ASTM D150
Chemical Properties Metric English Comments
Acid Value 2.0
2.0
[mgKOH/g}
Descriptive Properties Value Comments
Appearance Opaque white
Hydroxyl Value 3.5 mgKOH/g