Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

The NanoSteel® Company SHS 9700 GMAW OAW Steel Alloy, Cored Wire

Category Metal , Ferrous Metal , Alloy Steel , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer The NanoSteel® Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF The NanoSteel® Company SHS 9700 GMAW OAW Steel Alloy, Cored Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coating Description: SHS 9700 GMAW OAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that features exceptional abrasive wear resistance with superior toughness and no high-cost nickel, tungsten and molybdenum in material chemistry.Key Performance Characteristics67 - 70 HRc single and double pass weld depositsCost effective alternative to complex carbides: iron-based chemistry contains no tungsten, no molybdenum and no nickelProvides exceptional wear resistance lasting significantly longer than most chrome carbide and complex carbide alloysHigh resistance to abrasion while maintaining high toughnessCrystalline microstructure is engineered to submicron (400 nm) sizeMaintains high hardness after exposure to high temperaturesApplication Process: GMAW OAW Weld Overlay for HardfacingInformation Provided by The NanoSteel Company, Inc.
Physical Properties Metric English Comments
Density 7.36 g/cc
0.266 lb/in³
Weld Deposit Property
Mechanical Properties Metric English Comments
Hardness, Rockwell C 67 - 70
67 - 70
Component Elements Properties Metric English Comments
Aluminum, Al <= 5.0 %
<= 5.0 %
Boron, B <= 6.0 %
<= 6.0 %
Carbon, C <= 2.0 %
<= 2.0 %
Chromium, Cr <= 18 %
<= 18 %
Iron, Fe >= 60 %
>= 60 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Niobium, Nb (Columbium, Cb) <= 5.0 %
<= 5.0 %
Silicon, Si <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Impact Resistance Passed multiple impacts at 165 ft-lbs
Drop Impact Testing
Wear Resistance Mass Loss (g) 0.09-0.17
6000 cycles; ASTM G65-04 Procedure A
Users viewing this material also viewed the following: