Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
ASTM D2240
Tensile Strength, Yield 11.4 MPa
1650 psi
ASTM D412
Elongation at Break 690 %
690 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous; UL-1581
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Oxygen Index 23 %
23 %
ASTM D2863