Teknor Apex APEX® 91-A1386C-63NT Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 91-A1386C-63NT Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: RoHS Compliant Uses: Medical/Healthcare Applications Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
15 seconds; ASTM D2240
Tensile Strength at Break 12.5 MPa
1810 psi
ASTM D638
Elongation at Break 370 %
370 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous; ASTM D794
Descriptive Properties Value Comments
Appearance Clear