Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex APEX® 03-A0673C-85 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 03-A0673C-85 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 75°C Jacket; RoHS CompliantFeatures: Low Temperature Flexibility Uses: Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 719Forms: Pellets Wire Types: NMB; NMProcessing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
10 seconds; ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
ASTM D638
Elongation at Break 290 %
290 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Continuous Use; ASTM D794
Brittleness Temperature -32.0 °C
-25.6 °F
ASTM D746
Oxygen Index 22 %
22 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: