TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Poly AC 617A1.0MBTS4.0MBT2.0Thanecure® ZM1.0TP-9510.0Sulfur2.0Oyster Shell Calcium Carbonate40All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Tensile Strength, Yield 24.40 MPa
3539 psi
Elongation at Yield 687 %
687 %
100% Modulus 0.00165 GPa
0.239 ksi
200% Modulus 0.00250 GPa
0.362 ksi
300% Modulus 0.00355 GPa
0.515 ksi
Tear Strength 38.5 kN/m
220 pli
Taber Abrasion, mg/1000 Cycles 19

@Load 1.00 kg
19

@Load 2.20 lb
H-18 wheel
Compression Set 66.8 %

@Temperature 70.0 °C,
Time 79200 sec
66.8 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F