TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-326 (HS-HAF)

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-326 (HS-HAF).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Poly AC 617A1.0TP-9510.0Thanecure® ZM1.0MBTS4.0MBT2.0Sulfur1.5N-32620All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
Tensile Strength, Yield 31.34 MPa
4546 psi
Elongation at Yield 766 %
766 %
100% Modulus 0.00151 GPa
0.219 ksi
200% Modulus 0.00282 GPa
0.409 ksi
300% Modulus 0.007391 GPa
1.072 ksi
Tear Strength 53.6 kN/m
306 pli
Taber Abrasion, mg/1000 Cycles 6.0

@Load 1.00 kg
6.0

@Load 2.20 lb
H-18 wheel
Compression Set 53.8 %

@Temperature 70.0 °C,
Time 79200 sec
53.8 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 11.0 min

@Temperature 154 °C
0.183 hour

@Temperature 309 °F