Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 seconds
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Elongation at Break 465 %
465 %
Tear Strength Test 180
180
Processing Properties Metric English Comments
Melt Temperature 154 - 166 °C
310 - 330 °F