Stir SpA HE AT (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Stir SpA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA HE AT (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Extrusion various profiles for interior non-toxicInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.545 g/cc
0.05582 lb/in³
ISO 1183