Solvay Specialty Polymers Diofan® A 610 Polyvinylidene Chloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Diofan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 610 Polyvinylidene Chloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Diofan® A 610 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features exceptional barrier properties to water vapor and oxygen.Diofan® A 610 is a high surface tension latex; the addition of a convenient surfactant will enable to obtain a good quality coating as well as the addition of a coalescent agent to facilitate film formation at low temperature (< 10°C).Features: Flame Retardant; Moisture Barrier; Non-Toxic; Oxygen BarrierUses: Barrier Coatings; Coating ApplicationsAdditional Properties: Density - 1.650 g/cm³; Density - 1.330 g/cm³; Emulsion Type - Anionic; Filmability - 11 °C; Oxygen Transmission Rate - ASTM D3985 40 cm³/m²/bar/24 hr; pH - 1.5; Shelf Life - 10 month; Solids Content - 60 %; Surface Tension - 54 mN/mInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Water Vapor Transmission 14.0 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
0.902 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 16.0 °C
60.8 °F
DSC
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH); EU No 10/2011
Availability Asia Pacific
Europe
Latin America
North America
Color Milky White
Form Liquid