Solvay SOPROPHOR® TS/29 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name SOPROPHOR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay SOPROPHOR® TS/29 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED TRISTYRYLPHENOLCAS: 104376 – 75 – 2Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North America Applications: Multipurpose emulsifier, dispersing agent.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc

@Temperature 50.0 °C
0.0394 lb/in³

@Temperature 122 °F
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 45.0 °C
113 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Solid
Cloud Point 65.5-67.5°C
1% in NaCl 10%, RPG08
Composition Active
1
Ionic Charge Nonionic