Solvay RHODAFAC® PA32 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAFAC® PA32 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: ETHOXYLATED FATTY ALCOHOL, PHOSPHATE ESTERCAS: 106233 – 09 – 4Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Excellent extreme-pressure and anti-wear additive for industrial lubricants (rolling oils, hydraulic fluids, cutting fluids). Provides corrosion protection. Biodegradable and non ecotoxic surfactant.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Thermal Properties Metric English Comments
Melting Point 23.0 °C
73.4 °F
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Gardner Color Number <= 6.0
<= 6.0
RPG18
Chemical Properties Metric English Comments
Total Acid Number 88 - 94
88 - 94
[mg KOH/g], #1; RPG44
175 - 185
175 - 185
[mg KOH/g], #2; RPG44
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RPG16
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Paste
Composition Active
100
Ionic Charge Anionic