Material Notes:
Description: Alkyl etherhydroxypropyl sultaine. Non-foaming and protein defoaming wetting agent. Soluble and compatible in 50% caustic soda and high acid levels.Chemical Name: ALKYLETHER HYDROXYPROPYL SULTAINECAS: 108797-84-8, 108797-85-9Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: MIRATAINE ASC is intended for use in both alkaline and acid products where its extremely low foam, ease of handling and effective surface tension lowering will be of significant interestInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 49 - 51 %
49 - 51 %
Moisture Balance; RP-0536
pH 7.5 - 9.5
7.5 - 9.5
RP-0420
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Color <400
APHA, RP-1320
Composition Sodium Chloride
<8%, RP-0097
Ross Miles Foam Test 10 mm
1.0% Solution
5 mm
1.0% Solution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved