Material Notes:
Product Description: Mackazoline T is a fatty amine which, when neutralized with common acids, will act as a cationic surface active agent and emulsifier. It is oil soluble and water dispersible and contains no solvents. Mackazoline T offers good emulsification properties and stability. It can also be combined with alkyl halides and sulfates to form quaternary ammonium compounds. INCI Name: Tall Oil Hydroxyethyl Imidazoline CAS: 61791-39-7 EINECS: 263-171-2 Uses: Corrosion Inhibitors, Emulsifier and Oil Field Chemical SpecialtiesInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.920 - 0.940 g/cc
0.0332 - 0.0340 lb/in³
pH 10.5 - 11.5
10.5 - 11.5
10% Aqueous
Optical Properties Metric English Comments
Gardner Color Number <= 16
<= 16
Chemical Properties Metric English Comments
Total Acid Number <= 1.0
<= 1.0
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Amine Number
160-180
Imidazoline
>87%, MW 350