Material Notes:
Product Description: Mackam 50-SB is a high performance zwitterionic surfactant that has excellent lime soap dispersing properties and is stable over a wide pH range. It is compatible with anionic, nonionic, amphoteric and cationic surfactants. This grade of cocamidopropyl hydroxysultaine has a particularly low color and odor. Mackam 50-SB exhibits high foaming even in high electrolyte solutions. When compared to cocamidopropyl betaine, Mackam 50-SB exhibits better flash foam and viscosity-building characteristics with lauryl sulfates and alpha olefin sulfonates. Mackam 50-SB is produced from a high grade of purified, hydrogenated coco fatty acid and is fully biodegradable. It is stable in both hard and soft water. A glycerine-free grade that works well for quality mild shampoos, high-foaming bath products and liquid soaps. INCI NAME: Cocamidopropyl Hydroxysultaine CAS: 691400-36-9 Infrared Spectrum: Matches StandardUses: Shampoos, Body cleaners, Bubble Baths, Liquid Soaps, Lime soap dispersion and Oil field productsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Solids Content 48 - 51 %

@Temperature 105 °C,
Time 3600 sec
48 - 51 %

@Temperature 221 °F,
Time 1.00 hour
Oven
pH 7.0 - 9.0
7.0 - 9.0
10% Aqueous Sol'n
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Sodium Chloride
5.5-7.0%
Total Plate Count
<10 cfu/g
Odor Typical