Material Notes:
Identification: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHEDCAS: 68412 – 54 – 4Product Darkens with Prolonged Heating.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL CO-970 is a versatile emulsion polymerization surfactants and latex post stabilizers. Can be used as both sole-emulsifier and co-emulsifier.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Hard Waxy Solid
RP-0064
Color <100
APHA, RP-0134
Hydroxyl Number 32-27 mg KOH/g
RP-0245
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343