Solvay GEROPON® SS OIP LPH Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name GEROPON®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay GEROPON® SS OIP LPH Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: DISODIUM OLEOAMIDE (MIPA) SULFOSUCCINATECAS: 67815-88-7 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: GEROPON® SS-OIP/LPH is an anionic surfactant for emulsion polymerizationInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 36 - 39 %

@Temperature 110 °C,
Time 7200 sec
36 - 39 %

@Temperature 230 °F,
Time 2.00 hour
Oven; RP-0541
pH 5.5 - 6.4
5.5 - 6.4
1% Solution; RP-0420
Optical Properties Metric English Comments
Gardner Color Number <= 9.0
<= 9.0
RP-0138
Processing Properties Metric English Comments
Moisture Content 61 - 64 %
61 - 64 %
Karl Fisher; RP-0325
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear liquid
Composition Sodium Sulfite
<0.5%, EQ. WT. 63, RP-0522
Ionic Charge Anionic