Solvay Engineered Polymers DEXFLEX® 880-1 TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers DEXFLEX® 880-1 TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: DEXFLEX® 880-1 is a thermoplastic olefinic elastomer (TPO) designed for exterior automotive applications requiring a combination of stiffness, low-temperature impact, good processability, excellent paint durability, and excellent weatherability. Applications: Bumper fascias and other large components requiring durable paintability in exterior body colors. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
after bake; ISO 294
Melt Flow 13 g/10 min
13 g/10 min
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
2 in/min; ASTM D638
Flexural Modulus 0.725 GPa
105 ksi
I.B., TAN, 0.5 in/min; ASTM D790