Material Notes:
Description: A high purity alkanolamide that provides viscosity build, foam boosting, and emulsion stabilization.INCI NAME: Cocamide MEACAS: 68140-00-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMIDE® CME is a high purity alkanolamide that adds opacity, thickening, foam boosting, foam stabilization and mildness to shampoos, liquid soaps, bar soaps and body washes.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 8.0 - 10
8.0 - 10
1% Solution; RP-0420
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Off-White Waxy Solid
RP-0064
Composition Free Fatty Acid
<0.5%, EQ. WT. 200, RP-0007
Free MEA
<1.0%, EQ. WT. 61, RP-0203