| Category | Other Engineering Material , Additive/Filler for Polymer |
| Manufacturer | Silberline |
| Trade Name | Silvet® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Silberline Silvet® 890-20-P.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | 20 µm | 20 µm | Before Conversion |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |
| Descriptive Properties | Value | Comments |
|---|---|---|
| % Carrier | 20 | |
| Carrier | Polymethylmethacrylate Resin |