Sibur SKS-30 ARKM-27 1st Group Oil-Filled Styrene-Butadiene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur SKS-30 ARKM-27 1st Group Oil-Filled Styrene-Butadiene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SBR 1712. For use in the tire industry for production of tire thread and other parts for tires, in the rubber technical industry for production of a wide assortment of rubber technical articles, and in the shoe industry for production of white an colored footwear.
Physical Properties Metric English Comments
Mooney Viscosity 47 - 57

@Temperature 100 °C
47 - 57

@Temperature 212 °F
ML 1-4
Ash <= 0.60 %
<= 0.60 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 22.0 MPa
>= 3190 psi
Elongation at Break 550 - 750 %
550 - 750 %
Chemical Properties Metric English Comments
Styrene Content 22 - 25 %
22 - 25 %
Descriptive Properties Value Comments
Loss During Drying <0.35%
Mass Share Adigol-2 0.8-1.5
Mass Share of A-Methyl Styrene 22-25%
Mass Share of Oil 26-29%
Mass Share of VS-1 0.3-0.7
Mass Share of VTS-150 1-0.4
Spread Flow Batch Error <±6 %