Material Notes:
Buna CB 24. It is used in tires and the rubber and asbestos technical industries. It is combined with natural butadiene-styrene rubbers in any ratio, which is very important during production of articles on this base. Rubbers produced on a base rubber are extremely resistant to wearing.
Physical Properties Metric English Comments
Mooney Viscosity 40 - 48

@Temperature 100 °C
40 - 48

@Temperature 212 °F
ML 1-4
Ash <= 0.60 %
<= 0.60 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 19.5 MPa
>= 2830 psi
Tensile Strength, Yield >= 8.301 MPa

@Strain 300 %
>= 1204 psi

@Strain 300 %
Elongation at Break >= 480 %
>= 480 %
Descriptive Properties Value Comments
Loss During Drying <0.5%
Mass Share Adigol-2 0.6-1%
Mass Share Agidol-1 0.4-1%
Mass Share of Copper <0.0002
Mass Share of Iron <0.006%
Spread Flow Batch Error <±8 %