Sibur SKD 1st Grade Butadiene Rubber (BR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur SKD 1st Grade Butadiene Rubber (BR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing.
Physical Properties Metric English Comments
Mooney Viscosity 40 - 50

@Temperature 100 °C
40 - 50

@Temperature 212 °F
ML 1-4
Ash <= 0.30 %
<= 0.30 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 19.1 MPa
>= 2770 psi
Tensile Strength, Yield >= 6.89 MPa

@Strain 300 %
>= 1000 psi

@Strain 300 %
Elongation at Break >= 480 %
>= 480 %
Descriptive Properties Value Comments
Loss During Drying <0.8%
Mass Share Agidol-1 0.4-1%
Mass Share of Iron <0.006%
Spread Flow Batch Error <±8 %