Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Solids Content 70 %
70 %
Particle Size 0.50 µm
0.50 µm
Viscosity Measure 5000 cSt
5000 cSt
Emulsion
40000 cSt
40000 cSt
Descriptive Properties Value Comments
Appearance Emulsion
Diluent (%) 20cs
Surfactant Non-ionic
Users viewing this material also viewed the following: