Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones X-21-5561 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones X-21-5561 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Viscosity Measurement 15 - 40
15 - 40
cs
Descriptive Properties Value Comments
Active (%) 65
Appearance Liquid
CS 30
Diluent (%) ID
Hardness, Shore A M, Rubber
INCI Trimethylsiloxysilicate (and) Isododecane
Users viewing this material also viewed the following: