Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Viscosity Measurement 1600
1600
cs
Optical Properties Metric English Comments
Refractive Index 1.446
1.446
Descriptive Properties Value Comments
Active (%) 100
Appearance Liquid
Cloud Point 35
Diluent (%) NA
HLB 7
INCI PEG/PPG-20/22 Butyl Ether Dimethicone