KE571U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending filler.Product Features: This product can be blended with KE541U, KE551U, KE561U, and KE581Ufor intermediate hardnesses. The choice between these bases will depend on specific requirements.Typical Applications: Roll covers.Diaphragms.O-rings and gaskets.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
DCBP Cure
1.22 g/cc
1.22 g/cc
DBPH Cure
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
DCBP Cure
70
70
DBPH Cure
Tensile Strength at Break 10.80 MPa
1567 psi
DBPH Cure
11.20 MPa
1625 psi
DCBP Cure
Elongation at Break 370 %
370 %
DCBP Cure
440 %
440 %
DBPH Cure
Tear Strength 11.2 kN/m
64.0 pli
Die B; DCBP Cure
17.0 kN/m
97.0 pli
Die B; DBPH Cure
Compression Set 24 %

@Temperature 150 °C,
Time 79200 sec
24 %

@Temperature 302 °F,
Time 22.0 hour
DCBP Cure
Descriptive Properties Value Comments
Cure Agent DBPH
DCBP
Cure Type Post Cure