Sharadaa Ceramics MULL-SD Mullite

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Sharadaa Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics MULL-SD Mullite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rotary Kiln, Heat Curing and Acid Proof Lining Industry Focuses: Steel, Sponge, Rolling Mills, Coke Oven, Ferrous Foundries, Non-Ferrous, Cement, Petro Chemical, Mineral Processing, Sugar / Paper Mills and Chemical PlantsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 2.60 g/cc
0.0939 lb/in³
Porosity 16 - 18 %
16 - 18 %
Mechanical Properties Metric English Comments
Compressive Strength 78.5 MPa
11400 psi
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1650 °C
3000 °F
Component Elements Properties Metric English Comments
Al2O3 72 - 75 %
72 - 75 %
Fe2O3 0.20 %
0.20 %
Descriptive Properties Value Comments
PCE Orton 38
Permanent Linear Change -0.2 - 0.2%
1600°C