Sekisui PIOCELAN LSP-30EB Moldable Polymer Foam

Category Polymer , Thermoplastic , Polyolefin , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Sekisui Plastics
Trade Name PIOCELAN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sekisui PIOCELAN LSP-30EB Moldable Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: Packing material/Returnable containers for electronic parts and Automotive partsInformation provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.5706 MPa
82.76 psi
ASTM D3575
Elongation at Break 12.5 %
12.5 %
ASTM D3575
Flexural Strength 0.3367 MPa
48.83 psi
ASTM D790
Flexural Modulus 0.014309 GPa
2.0753 ksi
ASTM D790
Compressive Strength 0.2051 MPa

@Strain 25.0 %
29.74 psi

@Strain 25.0 %
ASTM D3575
0.2690 MPa

@Strain 50.0 %
39.01 psi

@Strain 50.0 %
ASTM D3575
0.5124 MPa

@Strain 75.0 %
74.32 psi

@Strain 75.0 %
ASTM D3575
Compression Set 38.8 %
38.8 %
ASTM D3575
Descriptive Properties Value Comments
Color Black
Range of center value of pre-expanded particles 0.1-0.15 in