Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Seals Eastern 5353 Nitrile Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Seals Eastern, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 5353 Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose NitrileInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 61
>= 61
ASTM D2240, Type A
70
70
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 12.63 MPa
>= 1832 psi
ASTM D412 Method A
19.69 MPa
2856 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield >= 1.10 MPa
>= 160 psi
Stress at Elongation M50; ASTM D412 Method A
1.23 MPa
179 psi
AVG Stress at Elongation M25; ASTM D412 Method A
1.68 MPa
244 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 1.71 MPa
>= 248 psi
Stress at Elongation M100; ASTM D412 Method A
2.94 MPa
426 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 321 %
>= 321 %
ASTM D412 Method A
424 %
424 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.000855 GPa
0.124 ksi
ASTM D412 Method A
Shear Modulus 0.00276 GPa
0.401 ksi
ASTM D412 Method A
Secant Modulus 0.007798 GPa
1.131 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 16