SK Chemicals SKYTHANE® 460A T series Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® 460A T series Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
ASTM D2240
Tensile Strength, Ultimate 17.7 MPa
2560 psi
ASTM D412
Tensile Strength, Yield 2.26 MPa

@Strain 100 %
327 psi

@Strain 100 %
ASTM D412
4.41 MPa

@Strain 300 %
640 psi

@Strain 300 %
ASTM D412
Elongation at Break 1200 %
1200 %
ASTM D412
Tear Strength 63.7 kN/m
364 pli
ASTM D624