Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: High Volume SealsCertified for use in potable water and/or in foodstuffInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
Open Porosity <= 2.5 %
<= 2.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
Size/Load - 10/100
Hardness, Shore C 86
86
Modulus of Elasticity 22.1 GPa
3200 ksi
Flexural Strength 58.6 MPa
8500 psi
Compressive Strength 159 MPa
23000 psi
Thermal Properties Metric English Comments
CTE, linear 6.48 µm/m-°C

@Temperature 20.0 °C
3.60 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 17.3 W/m-K
120 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
In oxygen
Maximum Service Temperature, Inert 204 °C
399 °F
Reducing Atm.
Descriptive Properties Value Comments
Impregnation Resin