S&E Specialty Polymers SE900-5 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers SE900-5 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Core which meets the Ford WSKM4D689-A4Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity <= 1.45 g/cc
<= 1.45 g/cc
ASTM D792, A
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 98

@Time 15.0 sec
90 - 98

@Time 0.00417 hour
ASTM D2240
Tensile Strength >= 16.0 MPa
>= 2320 psi
Type IV, 500mm/min; ASTM D638
Elongation at Break >= 150 %
>= 150 %
Type IV, 500mm/min; ASTM D638
Tear Strength >= 70.0 kN/m
>= 399 pli
Method B; ISO 34
Descriptive Properties Value Comments
Accelerated Weathering <3.0 DE
after 2000 kj/m<sup>2</sup>, SAEJ2527
Cold Flex -30°C
FLTM BN 102-01